| ITEM | STANDARD | TEST RESULT | 
| Melt Flow Rate @190C,2.16 (PERIODIC TEST)Kg,g/10min | ISO 1133 | 1.7 | 2.5       | 2.2 | 
| Notched Charpy Impact Str @23C kJ/m² | ISO 179/1eA | 12.0 | 18.0 | 15.2 | 
| Tensile Modulus,Mpa | ISO 527-1&2 | 2800 | 3200 | 2955 | 
| Tensile Stress @Yield,50 mm/min,MPa | ISO 527 | 70 | 75 | 73 | 
 
 
Key Properties
 
Mechanical Performance:
High stiffness, toughness, and creep resistance.
Excellent fatigue endurance for dynamic parts (e.g., gears, springs).
Low coefficient of friction, suitable for sliding/rotating components.
 
Thermal Stability:
Continuous service temperature: Up to 85°C (185°F).
Retains mechanical properties in sub-zero environments.
 
Chemical Resistance:
Resistant to hydrocarbons, alcohols, and many organic solvents.
Not recommended for strong acids, bases, or chlorine-rich environments.
 
Dimensional Stability:
Low moisture absorption (<0.2%), ensuring tight tolerances in humid conditions.
 
Machinability:
Easily machined into complex shapes with CNC or traditional tools.